Product overview
Dayu®SBS elastomer modified asphalt waterproofing membrane is a hot-melt waterproofing membrane composed of tire base, modified asphalt gum and surface material.
l fetal baseHigh quality filament polyester felt.
l Glial: Thermoplastic elastic rubber (styrene-butadiene-styrene) as a modifier to modify the petroleum asphalt (improve its high and low temperature performance, fatigue resistance), prepared into a dip coating gum, evenly coated on both sides of the tire base.
l Surface materialPolyethylene film, fine sandorMineral pellets.
Product Features
l High tensile strength, strong tear resistance, good dimensional stability and excellent mechanical properties.
l Excellent resistance to high and low temperature performance, low temperature not brittle crack, high temperature does not flow, good durability, long-term protection of waterproof ability.
l Mature hot melt method construction process, molten asphalt body lap, reliable bonding, lap firmly, suitable for all seasons.
l It can form a composite waterproof layer with other compatible coatings or coils to meet higher grade waterproof requirements.
Specification classification
Upper surface material |
Polyethylene film (PE)/S (fine sand)/M (mineral pellets) |
Thickness |
3.0 mm / 4.0 mm |
Width |
1000 mm |
Length |
7.5 m / 10 m |
Scope of application
l It is suitable for industrial, civil, municipal and other construction projects, including administrative, residential, commercial, scientific research, medical, school, grain depot, pipe gallery and other buildings.
l Applicable to the construction of underground works, roofing works. Wherein, the surface material of mineral grains can be used for non-human roof exposed waterproof.
ShiProcess
l Basic requirements: solid, dry, no sediment, laitance, no empty drum, loose, sand and other phenomena.
l Interface treatment: uniform spray (roll) coating matching base treatment agent, improve the coil and the adhesion of the base.
l Trial laying of coiled material: lay the coiled material flat on the base surface, align the elastic line or the overlapping edge of adjacent coiled material, adjust the overlapping width, and rewind after standing for a period of time to release the stress.
l Hot melt paving: bake the lower surface and base surface of the coil with a flame, push the roll-paving coil forward in time after the colloid is melted, and compact and exhaust while it is hot to tightly bond the coil with the base layer.
l Ontology lap joint: paving and pasting synchronous rolling lap joint edge until 5~8mm molten asphalt is extruded (regarded as reliable lap joint).
performance index
Products in accordance with the national standard "elastomer modified asphalt waterproofing membrane" GB18242-2008 manufacturing.
The material performance meets the standard requirements, and the complete index is detailed in the standard.
List of basic physical performance indicators of polyester base coil:
Project |
Indicator (Type I) |
Indicator (Type II) |
Soluble content |
≥ 2100g/㎡(3mm) ≥ 2900G/㎡(4mm) |
≥ 2100g/㎡(3mm) ≥ 2900G/㎡(4mm) |
Heat resistance |
No flowing or dripping at 90 ℃, slippage ≤ 2mm |
No flowing or dripping at 105 ℃, slippage ≤ 2mm |
Low temperature flexibility |
No crack at -20 ℃ |
No crack at -25 ℃ |
impervious to water |
0.3MPa, impervious to water for 120min |
0.3MPa, impervious to water for 120min |
Pull force |
≥ 500N/50mm |
≥ 800N/50mm |
Elongation |
≥30% |
≥40% |
Joint peel strength |
≥ 1.5N/mm |
≥ 1.5N/mm |
Previous Page