Product overview
Dayu®APP plastic body modified asphalt waterproofing membrane, is a hot melt waterproof membrane composed of tire base, plastic body modified asphalt gum, surface material.
l fetal baseHigh quality filament polyester felt.
l Glial: APP (random polypropylene) as a modifier to modify the petroleum asphalt, prepared into a dip coating gum, evenly coated on both sides of the tire base.
l Surface materialPolyethylene film, fine sandorMineral pellets.
Product Features
l High tensile strength, strong tear resistance, good dimensional stability, excellent mechanical properties, and strong resistance to breakage.
l Excellent high temperature resistance, high temperature 130 ℃ does not flow.
l Mature hot melt method construction process, molten asphalt body lap, reliable bonding, lap firmly, suitable for all seasons.
l It can form a composite waterproof layer with other compatible coatings or coils to meet higher grade waterproof requirements.
Specification classification
Upper surface material |
Polyethylene film (PE)/S (fine sand)/M (mineral pellets) |
Thickness |
3.0mm/4.0mm |
Width |
1000mm |
Length |
7.5m/10m |
Scope of application
l It is suitable for industrial, civil, municipal and other construction projects, including administrative, residential, commercial, scientific research, medical, school, grain depot, pipe gallery and other buildings.
l It is suitable for road and bridge waterproof engineering, high temperature industrial plant roof waterproof engineering, or roof waterproof engineering of buildings in high temperature areas in the south.
l The membrane with mineral granules can be used for exposed waterproofing of non-human roofs.
Construction process
L grass-roots requirements: solid, dry, free of sediment, laitance, no empty drum, loose, sand and other phenomena.
L interface treatment: uniform spray (roll) coating matching base treatment agent, improve the coil and the adhesion of the base.
L trial laying of coiled material: lay the coiled material flat on the base surface, align the elastic line or the overlapping edge of adjacent coiled material, adjust the overlapping width, let stand for a period of time to release the stress and then roll back.
L hot melt paving: bake the lower surface and base surface of the coil with a flame, push the roll paving coil forward in time after the colloid is melted, and compact and exhaust while it is hot to make the coil and the base closely bond.
L body lap joint: paving and pasting synchronous rolling lap joint edge to extrude 5~8mm molten asphalt (regarded as reliable lap joint).
performance index
Products in accordance with the national standard "plastic modified asphalt waterproofing membrane" GB18243-2008 manufacturing.
The material performance meets the standard requirements, and the complete index is detailed in the standard.
List of basic physical performance indicators of polyester base coil:
Project |
Indicator (Type I) |
Indicator (Type II) |
Soluble content |
≥ 2100g/㎡(3mm) ≥ 2900G/㎡(4mm) |
≥ 2100g/㎡(3mm) ≥ 2900G/㎡(4mm) |
Heat resistance |
No flowing or dripping at 110 ℃, slippage ≤ 2mm |
No flowing or dripping at 130 ℃, slippage ≤ 2mm |
Low temperature flexibility |
No crack at -7 ℃ |
No crack at -15 ℃ |
impervious to water |
0.3MPa, impervious to water for 30min |
0.3MPa, impervious to water for 30min |
Pull force |
≥ 500N/50mm |
≥ 800N/50mm |
Elongation |
≥25% |
≥40% |
Joint peel strength |
≥ 1.0N/mm |
≥ 1.0N/mm |